slicershare (test)

Bambu PPS-CF @base

Bambu Lab · PPS-CF · by bambu-system · 1 download

Inheritance

    fdm_filament_common fdm_filament_pps Bambu PPS-CF @base

Inherited from this (6)

Settings

Basic information

Material variant
PPS-CF overridden
was PPS (inherited)
Vendor
Bambu Lab overridden
was Generic (inherited)
Diameter (mm)
1.75 inherited
Density (g/cm³)
1.26 overridden
was 1.36 (inherited)
Cost (/kg)
175 overridden
was 0 (inherited)

Print temperature

Nozzle (initial layer) (°C)
320 inherited
Nozzle (other layers) (°C)
320 inherited

Cooling

Fan minimum (%)
0 inherited
Fan maximum (%)
30 overridden
was 50 (inherited)
Disable fan for first N layers
3 inherited
Full fan if layer below (sec)
5 inherited
Slow down if layer below (sec)
2 inherited
Min speed when slowed (mm/s)
10 inherited

Flow

Flow ratio
0.96 inherited
Max volumetric speed (mm³/s)
6 overridden
was 4 (inherited)

Retraction

Retraction length (mm)
nil inherited
Retraction speed (mm/s)
nil inherited
Deretraction speed (mm/s)
nil inherited

Bed temperature

Plate Initial layer (°C) Other layers (°C)
Cool Plate
0 inherited
0 inherited
Engineering Plate
110 inherited
110 inherited
High Temp Plate
110 inherited
110 inherited
Textured PEI Plate
110 inherited
110 inherited
Cool Plate SuperTack
0 inherited
0 inherited

Other settings

additional fan full speed layer
0 inherited
chamber temperatures
60 inherited
close additional fan first x layers
3 inherited
description
When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials. overridden
filament adhesiveness category
801 inherited
filament dev ams drying ams limitations
-1 inherited
filament dev ams drying heat distortion temperature
165 inherited
filament dev ams drying temperature
65, 85, 65, 85 inherited
filament dev ams drying time
12, 12, 12, 12 inherited
filament dev chamber drying bed temperature
100 inherited
filament dev drying cooling temperature
150 inherited
filament dev drying softening temperature
150 inherited
filament id
GFT02 overridden
filament is support
0 inherited
filament minimal purge on wipe tower
15 inherited
filament retract before wipe
nil inherited
filament retract restart extra
nil inherited
filament retract when changing layer
nil inherited
filament retraction minimum travel
nil inherited
filament soluble
0 inherited
filament wipe
nil inherited
filament wipe distance
nil inherited
filament z hop
nil inherited
full fan speed layer
0 inherited
impact strength z
2.8 overridden
instantiation
false overridden
was false (inherited)
nozzle temperature range high
340 inherited
nozzle temperature range low
310 overridden
was 300 (inherited)
overhang fan speed
30 inherited
overhang fan threshold
25% overridden
was 0% (inherited)
reduce fan stop start freq
0 inherited
required nozzle HRC
40 overridden
was 3 (inherited)
slow down for layer cooling
1 inherited
temperature vitrification
220 overridden
was 125 (inherited)
  1. v1 created 2026-05-19 04:15