Ultrafuse PA
BASF · NYLON
· by super-system
· 0 downloads
Inheritance
-
*common*
→
Fillamentum Nylon FX256
→
Ultrafuse PA
Inherited from this (1)
Settings
Basic information
- Material variant
-
NYLON inherited
- Vendor
-
BASF overriddenwas Fillamentum (inherited)
- Diameter (mm)
-
1.75 inherited
- Density (g/cm³)
-
1.12 overriddenwas 1.01 (inherited)
- Cost (/kg)
-
0 overriddenwas 56.99 (inherited)
Print temperature
- Nozzle (initial layer) (°C)
-
240 overriddenwas 250 (inherited)
- Nozzle (other layers) (°C)
-
240 overriddenwas 250 (inherited)
Cooling
- Fan minimum (%)
-
0 overriddenwas 0 (inherited)
- Fan maximum (%)
-
0 overriddenwas 0 (inherited)
- Disable fan for first N layers
-
6 inherited
- Full fan if layer below (sec)
-
30 overriddenwas 20 (inherited)
- Slow down if layer below (sec)
-
20 overriddenwas 20 (inherited)
- Min speed when slowed (mm/s)
-
15 overriddenwas 15 (inherited)
Flow
- Flow ratio
-
1 inherited
- Max volumetric speed (mm³/s)
-
11 overriddenwas 6 (inherited)
Bed temperature
| Plate | Initial layer (°C) | Other layers (°C) |
|---|---|---|
| High Temp Plate |
80
overridden
was 90
|
70
overridden
was 90
|
Other settings
- bridge fan speed
-
0 overriddenwas 30 (inherited)
- compatible printers condition
-
printer_model!="MINI" and printer_model!="MK2SMM" and ! (printer_notes=~/.*PRINTER_VENDOR_PRUSA3D.*/ and printer_notes=~/.*PRINTER_MODEL_MK(2.5|3).*/ and single_extruder_multi_material) overriddenwas — (inherited)
- cooling
-
1 inherited
- fan always on
-
0 inherited
- filament colour
-
#ECFAFF overriddenwas #DEE0E6 (inherited)
- filament cooling final speed
-
3.4 inherited
- filament cooling initial speed
-
2.2 inherited
- filament cooling moves
-
4 inherited
- filament load time
-
0 inherited
- filament loading speed
-
28 inherited
- filament loading speed start
-
3 inherited
- filament minimal purge on wipe tower
-
15 inherited
- filament notes
-
Material Description The key features of Ultrafuse PA are the high strength and high modulus. Furthermore, Ultrafuse PA shows a good thermal distortion stability. Printing Recommendations: Apply PVA glue, Kapton tape or PA adhesive to a clean buildplate to improve adhesion. overriddenwas — (inherited)
- filament ramming parameters
-
120 100 6.6 6.8 7.2 7.6 7.9 8.2 8.7 9.4 9.9 10.0| 0.05 6.6 0.45 6.8 0.95 7.8 1.45 8.3 1.95 9.7 2.45 10 2.95 7.6 3.45 7.6 3.95 7.6 4.45 7.6 4.95 7.6 inherited
- filament retract before travel
-
2 overridden
- filament retract layer change
-
0 overridden
- filament retract length
-
1 overridden
- filament retract lift
-
0 overridden
- filament soluble
-
0 inherited
- filament spool weight
-
0 overriddenwas 230 (inherited)
- filament toolchange delay
-
0 inherited
- filament unload time
-
0 inherited
- filament unloading speed
-
90 inherited
- filament unloading speed start
-
100 inherited
- start filament gcode
-
M900 K{if printer_notes=~/.*PRINTER_MODEL_MINI.*/ and nozzle_diameter[0]==0.6}0.12{elsif printer_notes=~/.*PRINTER_MODEL_MINI.*/ and nozzle_diameter[0]==0.8}0.06{elsif printer_notes=~/.*PRINTER_MODEL_MINI.*/}0.2{elsif nozzle_diameter[0]==0.8}0.01{elsif nozzle_diameter[0]==0.6}0.02{else}0.04{endif} ; Filament gcode LA 1.5 {if printer_notes=~/.*PRINTER_MODEL_MINI.*/};{elsif printer_notes=~/.*PRINTER_HAS_BOWDEN.*/}M900 K200{elsif nozzle_diameter[0]==0.6}M900 K12{elsif nozzle_diameter[0]==0.8};{else}M900 K20{endif} ; Filament gcode LA 1.0 overriddenwas M900 K{if printer_notes=~/.*PRINTER_MODEL_MINI.*/ and nozzle_diameter[0]==0.6}0.12{elsif printer_notes=~/.*PRINTER_MODEL_MINI.*/ and nozzle_diameter[0]==0.8}0.06{elsif printer_notes=~/.*PRINTER_MODEL_MINI.*/}0.2{elsif nozzle_diameter[0]==0.8}0.02{elsif nozzle_diameter[0]==0.6}0.05{else}0.1{endif} ; Filament gcode LA 1.5 {if printer_notes=~/.*PRINTER_MODEL_MINI.*/};{elsif printer_notes=~/.*PRINTER_HAS_BOWDEN.*/}M900 K200{elsif nozzle_diameter[0]==0.6}M900 K28{elsif nozzle_diameter[0]==0.8};{else}M900 K48{endif} ; Filament gcode LA 1.0 (inherited)
Raw resolved JSON
{
"cooling": [
"1"
],
"filament_cost": [
"0"
],
"filament_notes": [
"Material Description\nThe key features of Ultrafuse PA are the high strength and high modulus. Furthermore, Ultrafuse PA shows a good thermal distortion stability.\n\nPrinting Recommendations:\nApply PVA glue, Kapton tape or PA adhesive to a clean buildplate to improve adhesion."
],
"filament_density": [
"1.12"
],
"filament_soluble": [
"0"
],
"filament_diameter": [
"1.75"
],
"end_filament_gcode": [
""
],
"filament_load_time": [
"0"
],
"compatible_printers": [
""
],
"filament_flow_ratio": [
"1"
],
"slow_down_min_speed": [
"15"
],
"filament_settings_id": [
""
],
"filament_unload_time": [
"0"
],
"slow_down_layer_time": [
"20"
],
"start_filament_gcode": [
"M900 K{if printer_notes=~/.*PRINTER_MODEL_MINI.*/ and nozzle_diameter[0]==0.6}0.12{elsif printer_notes=~/.*PRINTER_MODEL_MINI.*/ and nozzle_diameter[0]==0.8}0.06{elsif printer_notes=~/.*PRINTER_MODEL_MINI.*/}0.2{elsif nozzle_diameter[0]==0.8}0.01{elsif nozzle_diameter[0]==0.6}0.02{else}0.04{endif} ; Filament gcode LA 1.5\n{if printer_notes=~/.*PRINTER_MODEL_MINI.*/};{elsif printer_notes=~/.*PRINTER_HAS_BOWDEN.*/}M900 K200{elsif nozzle_diameter[0]==0.6}M900 K12{elsif nozzle_diameter[0]==0.8};{else}M900 K20{endif} ; Filament gcode LA 1.0"
],
"filament_cooling_moves": [
"4"
],
"filament_loading_speed": [
"28"
],
"filament_unloading_speed": [
"90"
],
"filament_toolchange_delay": [
"0"
],
"filament_ramming_parameters": [
"120 100 6.6 6.8 7.2 7.6 7.9 8.2 8.7 9.4 9.9 10.0| 0.05 6.6 0.45 6.8 0.95 7.8 1.45 8.3 1.95 9.7 2.45 10 2.95 7.6 3.45 7.6 3.95 7.6 4.45 7.6 4.95 7.6"
],
"filament_cooling_final_speed": [
"3.4"
],
"filament_loading_speed_start": [
"3"
],
"compatible_printers_condition": [
"printer_model!=\"MINI\" and printer_model!=\"MK2SMM\" and ! (printer_notes=~/.*PRINTER_VENDOR_PRUSA3D.*/ and printer_notes=~/.*PRINTER_MODEL_MK(2.5|3).*/ and single_extruder_multi_material)"
],
"filament_cooling_initial_speed": [
"2.2"
],
"filament_unloading_speed_start": [
"100"
],
"filament_minimal_purge_on_wipe_tower": [
"15"
],
"fan_always_on": [
"0"
],
"fan_max_speed": [
"0"
],
"fan_min_speed": [
"0"
],
"filament_type": [
"NYLON"
],
"hot_plate_temp": [
"70"
],
"filament_colour": [
"#ECFAFF"
],
"filament_vendor": [
"BASF"
],
"bridge_fan_speed": [
"0"
],
"nozzle_temperature": [
"240"
],
"filament_spool_weight": [
"0"
],
"fan_cooling_layer_time": [
"30"
],
"close_fan_the_first_x_layers": [
"6"
],
"hot_plate_temp_initial_layer": [
"80"
],
"filament_max_volumetric_speed": [
"11"
],
"nozzle_temperature_initial_layer": [
"240"
],
"filament_retract_lift": [
"0"
],
"filament_retract_length": [
"1"
],
"filament_retract_layer_change": [
"0"
],
"filament_retract_before_travel": [
"2"
],
"name": "Ultrafuse PA",
"type": "filament"
}